Aluminium 2014 Sheets and Plates Description
2014 is a heat-treatable aluminium-copper-magnesium-silicon alloy. Copper (3.9–5.0%) is the principal alloying element; magnesium and silicon combine to form the precipitates that carry the strength after heat treatment, and manganese refines the grain.
The silicon is what separates 2014 from 2024. It improves forgeability, which is why 2014 is also a forging alloy, and it pushes tensile strength higher in T6 and T651 plate.
As with other 2xxx alloys, the strength comes at the cost of corrosion resistance and weldability. Both need to be designed around rather than discovered later.
Chemical composition of 2014 aluminum
The alloy is registered under two slightly different composition sets: the Aluminium Association designation used with ASTM B209, and EN AW-2014A used with EN 573-3. They differ mainly in silicon range, iron limit and whether nickel and Ti+Zr are controlled. Both are listed below because the correct set depends on which standard governs your order.
| 2014 (AA / ASTM B209) | EN AW-2014A (EN 573-3) | |
|---|---|---|
| 0.50 – 1.2 | 0.50 – 0.90 | |
| <= 0.70 | <= 0.50 | |
| 3.9 – 5.0 | 3.9 – 5.0 | |
| 0.40 – 1.2 | 0.40 – 1.2 | |
| 0.20 – 0.80 | 0.20 – 0.80 | |
| <= 0.25 | <= 0.25 | |
| <= 0.15 | <= 0.15 | |
| <= 0.10 | <= 0.10 | |
| <= 0.10 | ||
| Titanium + Zirconium (Ti+Zr) | <= 0.20 | |
| <= 0.05 / <= 0.15 | <= 0.05 / <= 0.15 | |
State the governing standard (ASTM B209 or EN 573-3) with the inquiry so the correct composition set is certified.
Mechanical properties of 2014 aluminum by temper
2014 covers a wide strength band depending on heat treatment. Minimum values below are the specification figures; typical values are what production material commonly measures.
| Yield 0.2%, MPa | |||
|---|---|---|---|
| 2014-O | <= 220 max; typical 185 | ~95 – 100 | 12 – 16 |
| 2014-T4 | 370 – 425 min; typical 425 | 225 – 290 min; typical 290 | 10 – 18 |
| 2014-T451 | ~425 | ~290 | ~18 |
| 2014-T6 (sheet) | 440 min; typical 480 – 485 | 380 – 395 min; typical 415 | 6 – 11 |
| 2014-T651 (plate) | 450 – 460 min; typical 485 | 390 – 400 min; typical 415 | 7 – 11 |
Brinell hardness runs around 133–135 HB in T6 and 131–138 HB across T651 plate thicknesses, increasing with section size up to 40 mm.
Minimum and typical figures are drawn from ASTM B209 / EN 485-2 tables and published manufacturer data; values differ between sources and shift with thickness and test direction. The certificate for your heat and thickness governs.
Mechanical properties of 2014 aluminum plate by thickness
Strength in 2014 plate is graded by section thickness, because thick sections cannot be quenched and aged to the same condition as thin ones. Design to the band your plate falls in, not to the headline figure.
| Sheet 0.4 – 6.0 mm | 440 | 390 | - | 133 |
| Plate 6 – 12.5 mm | 450 | 395 | 7 (A50) | 135 |
| Plate 12.5 – 40 mm | 460 | 400 | 6 | 138 |
| Plate 40 – 60 mm | 450 | 390 | 5 | 135 |
| Plate 60 – 80 mm | 435 | 380 | 4 | 131 |
Values are for 2014 / 2014A in the T6 and T651 condition. Alclad sheet carries lower figures because the cladding layer carries less load; ask for the clad sheet table if your design uses it. Elongation is measured over the gauge length the standard specifies for each band.
Physical properties of 2014 aluminum
| 2.82 g/cm³ (some datasheets list 2.80) | |
| ~71 GPa (some datasheets list 73 GPa) | |
| Coefficient of thermal expansion, 20–100 ℃ | 23 ×10-6/K |
| 138 W/m·K | |
| 0.045 ×10-6 Ω·m | |
| ~507 – 638 ℃ | |
| 2.82 kg per mm per m² |
Density and modulus figures vary between datasheets; the values used for calculation should be stated on the drawing so everyone works to the same number.
Tempers of 2014 aluminum
| 2014-O | ||
| 2014-T3 | ||
| 2014-T4 | ||
| 2014-T451 | ||
| 2014-T6 | ||
| 2014-T651 | ||
| Alclad 2014 | Pure-aluminium layer bonded to the surface |
If a drawing simply says "2014 plate T6" but the part is heavily milled, ask whether T651 was intended. The difference shows up as distortion after machining, and it costs nothing to resolve before the order.
Applications of 2014 aluminum
2014 is specified where a component carries very high static loads and where its corrosion and welding limits can be managed:
- wing and fuselage members, frames, ribs and heavily loaded fittings
- the silicon content gives 2014 good forgeability; structural fittings, brackets and rings forged in the O condition and heat treated to T6 or T651 afterwards
- parts milled from solid in T6 or T651, where chip control and surface finish matter
- truck frames, suspension components and chassis reinforcements in high-load ground vehicles
- suspension arms, uprights, driveline components
- where dimensional stability after machining and high stiffness are required
- structural members and machined hardware
Comparison of 2014 aluminum with 2024, 6061 and 7075
Typical property ranges used to understand relative strength levels, from ASTM B209 / EN 485-2 and AMS data. They are selection reference; actual design calculations must use the guaranteed minimum values in the governing standard.
| 2014-T651 plate | 440 – 490 | 390 – 440 | 8 – 12 | High-load structure, tooling, machined plate |
| 2014-T6 sheet | 440 – 480 | 380 – 430 | 8 – 12 | |
| 2024-T351 plate | 430 – 480 | 320 – 360 | 10 – 20 | Aircraft skins, fatigue-critical structure |
| 6061-T651 plate | 260 – 320 | 240 – 280 | 10 – 17 | |
| 7075-T651 plate | 510 – 580 | 430 – 520 | 7 – 11 |
Read across the yield line rather than the tensile line: 2014 and 2024 sit at a similar level of tensile strength, but 2014 carries roughly 70 MPa more yield than 2024-T351, and roughly 160 MPa more than 6061-T651.
Machining, forging and joining of 2014 aluminum
2014 machines well in T6 and T651 with carbide tooling at moderate cutting speeds, producing acceptable chip formation and surface finish. It is not a free-machining alloy in the class of 2011, so chip breaking should be part of the tooling choice rather than assumed.
The silicon content gives 2014 good forgeability in the O and as-fabricated conditions. Forged shapes such as fittings, brackets and rings are produced first and then solution treated and aged to T6 or T651.
Riveting, bolting and adhesive bonding are the standard joining methods for 2014.
Fusion welding by TIG or MIG is not recommended. The copper-rich chemistry promotes hot cracking in the heat affected zone and welded joints show reduced properties. Where welding is unavoidable it needs a qualified procedure and filler selection; friction stir welding is the preferred route where a welded joint is essential.
Isolate 2014 from carbon steel and copper in mechanical joints; it is anodic to both.
Corrosion protection of 2014 aluminum
Bare 2014 has poor resistance to atmospheric attack, particularly where water or salt is present. Specify one of these routes and say which one when you inquire:
Alclad 2014 - a metallurgically bonded pure-aluminium layer; the standard approach for 2xxx aerospace sheet
- improves wear and corrosion resistance; note that high copper content gives a less uniform colour than 6xxx alloys
- applied to the coating supplier's preparation procedure
- a lanolin-based film for storage and transit protection of unclad material
Unclad 2014 left outdoors without a coating system is the failure mode that most often gets blamed on the supplier.
Specifications and supply range of 2014 aluminum
| Aluminium sheet and plate, alloy 2014 / 2014A | |
| O, T3, T4, T451, T6, T651; Alclad on request | |
| Sheet 0.4 – 6.0 mm; plate 6 – 150 mm; forged block on request | |
| 1000 – 2600 mm | |
| 2000 – 12000 mm, cut-to-length to your cut list | |
| Per ASTM B209 / EN 485-4; confirmed with the quote for your thickness and width | |
| Black and white, blue or transparent PE film, 50 or 80 micron | |
| ASTM B209 / ASME SB209, EN 485-2, EN 573-3, ISO 209, GB/T 3190; AMS numbers per drawing | |
| UNS A92014, EN AW-2014 / 2014A (AlCu4SiMg, 3.1255), ISO AlCu4SiMg, DIN AlCuSiMn, BS HE15, AFNOR A-U4SG, CSA CS41N, JIS A2014, GB 2A14 (formerly LD10) |
Dimensional ranges are common industry supply parameters, not a stock commitment; the orderable range for a given temper and thickness is confirmed with the quote.
Ordering 2014 aluminum sheet and plate
Send the alloy and governing standard, temper, thickness, width, length, quantity, surface or cladding requirement, certificate scope and destination port. Tell us whether the part will be heavily machined or joined, and we will confirm temper selection, certification, packing and schedule together.
| Flexible - trial and small orders are negotiable | |
| About 15 – 30 days from order confirmation | |
| EN 10204 3.1 standard; EN 10204 3.2 with third-party witness on request | |
| FOB, CIF, EXW - confirmed per order |
| 2014 / 2014A (UNS A92014, EN AW-2014, AlCu4SiMg) | |
| Listed under China's dual-use export control list (two-use items and technologies) | |
| Flat-rolled sheet and plate | |
| First-round screening result | Passed - flat-rolled 2014 is not a licensable-controlled export in this form |
| End-use statement and export declarations prepared per order and destination |
2014 is on the same dual-use list as other high-strength grades such as 2024, 7075, 7050, 2017, 7A04, 2195, 7068, 7055 and 7150. Their export status depends on product form and dimensions and is screened per enquiry. Note that 2014 bar, tube and forging are screened separately and may carry different conditions from the flat-rolled form on this page.
This is a screening statement, not a licence determination. As flat-rolled sheet and plate, 2014 clears first-round export screening and is exportable. We handle the export paperwork per order and destination.


GNEE has supplied aluminum products since 2008 and now exports to more than 100 countries and regions.
Common plate thicknesses and sheet sizes are held in stock so repeat and small orders ship without waiting for a rolling slot; non-standard widths, lengths and tempers are produced to order.
Order size is flexible - trial quantities and full containers are quoted on the same terms, so order the quantity you actually need rather than padding to a threshold.
Standard specifications are delivered in 15–30 days; we confirm the date against the current production schedule before you commit, not after.
Every shipment includes an EN 10204 3.1 mill test certificate, and 3.2 certification with third-party inspection (SGS, BV, TÜV and others) can be arranged when the project requires it.
Our sales engineers read your drawings and ask about load, environment and fabrication method before recommending a temper, and will tell you if a specification is wrong for the job.





What is 2014 aluminum used for?
2014 is used for highly stressed aerospace structural members, frames, ribs and fittings, forged components, truck frames and heavy vehicle suspension parts, performance automotive components, tooling and fixtures, and defence vehicle structures. It is chosen where very high strength and machinability matter more than corrosion resistance or weldability.
Can 2014 aluminium be welded?
Fusion welding is not recommended. The alloy is sensitive to hot cracking in the heat affected zone and welded joints show reduced properties. Join it by riveting, bolting or adhesive bonding, and use friction stir welding where a welded joint is essential and the procedure can be qualified.
What is the difference between 2014 and 2024 aluminium?
Both are heat-treatable aluminium-copper alloys. 2014 contains 0.5–0.9% silicon under the EN designation (up to 1.2% under the AA designation), which improves forgeability, while 2024 has no added silicon and is the established choice for aircraft skin sheet. 2014 reaches higher yield strength in T651 plate; 2024 is the established choice for fatigue-critical skins and thin sheet.
T651 for plate and T6 for sheet. Both are at peak strength and hardness, giving clean cutting, good chip control and a fine finish. T651 is stress relieved by stretching, so it moves less after heavy material removal - which is why it is preferred for heavily milled plate components.
Does 2014 need corrosion protection?
Yes. At 3.9–5.0% copper, bare 2014 is significantly less corrosion resistant than 5xxx or 6xxx alloys, particularly in water or salt environments. Specify Alclad cladding, anodizing, or a conversion coating plus paint system. Unclad 2014 should never be left exposed outdoors uncoated.
What mechanical properties does 2014-T651 plate have?
Minimum tensile strength is 450 MPa at 6–12.5 mm and 460 MPa at 12.5–40 mm, falling to 435 MPa at 60–80 mm. Minimum proof stress runs 380–400 MPa across the same bands, and elongation drops from 7% to 4% as thickness increases.
Which standards cover 2014 sheet and plate?
ASTM B209 / ASME SB209 covers sheet and plate; EN 485-2 covers mechanical properties and EN 573-3 composition for European supply; ISO 209 and GB/T 3190 cover designation and composition. Aerospace orders commonly reference AMS specifications - send the number from your drawing.
MOQ is flexible and trial quantities are negotiable. Lead time is about 15 to 30 days from order confirmation, depending on temper, thickness, quantity and certification scope.
Is 2014 aluminum sheet and plate export controlled?
2014 is listed under China's dual-use export control list. As flat-rolled sheet and plate it passes first-round export screening and is exportable; this is a screening statement, not a licence determination. We prepare end-use documentation and export declarations per order and destination. Bar, tube and forging forms of 2014 are screened separately and may carry different conditions.
Request a quote for 2014 aluminum sheet and plate
Send the alloy and governing standard, temper, thickness, width, length, quantity, surface or cladding requirement, certificate scope and destination port. Tell us whether the part will be heavily machined or joined, and we will confirm temper selection, certification, packing and schedule together.
Get a quote for 2014 aluminum sheet and plate
горячая этикетка : aluminium 2014 sheets and plates, China aluminium 2014 sheets and plates manufacturers
Предыдущая статья
Алюминиевый лист и пластины 2017 г.Следующая статья
Алюминиевая пластинаВам также может понравиться
Отправить запрос